PROBLEM TO BE SOLVED: To provide a method for adjusting the furnace temperature in a heating-combustion zone in a rotary-hearth furnace and the rotary-hearth furnace with which explosive cracking and brittleness of a material to be treated, in the heating-combustion zone in the rotary-hearth furnace, are prevented and also, the material to be treated can be uniformly heated.;SOLUTION: In the method for adjusting the furnace temperature in the rotary-hearth furnace, in which the material to be treated, charged into the rotary-hearth furnace 1, is heated and reduced at the heating-combustion zone 6 and a reducing-combustion zone 7 to produce a reduction iron; an exhaust gas exhausted from the rotary-hearth furnace, is cooled, and a part of the exhaust gas, removing dust in a dust-collector (temperature: 150-250°C; oxygen concentration: 2-10 vol%), is blown into the heating-combustion zone, to heat the material to be treated at 700-1,100°C.;COPYRIGHT: (C)2010,JPO&INPIT
机译:解决的问题:提供一种用于调节旋转式炉床炉和旋转式炉床的加热燃烧区中的炉温的方法,在加热燃烧区中,待处理材料的爆炸性破裂和脆性解决方案:在旋转式炉膛中调节炉温的方法中,将要处理的物料装入炉膛中进入旋转式炉床炉1中的加热燃烧区6和还原燃烧区7进行加热和还原以产生还原铁。从旋转式炉膛炉中排出的废气被冷却,并且吹出一部分废气,以除去集尘器中的灰尘(温度:150-25℃;氧气浓度:2-10vol%)。进入加热燃烧区,以700-1,100°C加热待处理物料;版权所有:(C)2010,JPO&INPIT

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号