首页> 外国专利> METHOD FOR PRODUCING SILICA-COATED GOLD COLLOIDAL PARTICLE, AND SILICA-COATED GOLD COLLOIDAL PARTICLE

METHOD FOR PRODUCING SILICA-COATED GOLD COLLOIDAL PARTICLE, AND SILICA-COATED GOLD COLLOIDAL PARTICLE

机译:二氧化硅包覆的金胶体粒子的制造方法以及二氧化硅包覆的金胶体粒子

摘要

PROBLEM TO BE SOLVED: To provide a silica-coated gold colloidal particle which is not flocculated or discolored even when heating treatment is applied, and capable of maintaining clear red.;SOLUTION: Disclosed is a method for producing a silica-coated gold colloidal particle characterized in that a gold colloidal particle (M)-dispersed liquid in which the average particle diameter lies in the range of 5 to 100 nm, and subjected to surface treatment with a carboxyl group and/or carboxylate group-containing organic compound and a silica colloidal particle (A)-dispersed liquid in which the average particle diameter lies in the range of 4 to 40 nm, and subjected to surface treatment with an amino group-containing silane compound are mixed. Also disclosed is a method for producing a silica-coated gold colloidal particle characterized in that a gold colloidal particle (M)-dispersed liquid in which the average particle diameter lies in the range of 5 to 100 nm and a silica colloidal particle (A)-dispersed liquid in which the average particle diameter lies in the range of 4 to 40 nm, and subjected to surface treatment with a mercapto group-containing silane compound, and into which a thiol group(-SH group) is introduced are mixed.;COPYRIGHT: (C)2009,JPO&INPIT
机译:解决的问题:提供一种即使在进行加热处理时也不会絮凝或变色并且能够保持清澈的红色的二氧化硅包覆的金胶体粒子;解决方案:本发明公开了一种二氧化硅包覆的金胶体粒子的制备方法。其特征在于,分散有平均粒径在5〜100nm的范围内的金胶体粒子(M)分散液,并用含羧基和/或羧基的有机化合物和二氧化硅进行了表面处理。将平均粒径为4〜40nm的胶体粒子(A)分散液混合,并用含氨基的硅烷化合物进行了表面处理。还公开了一种制备二氧化硅包覆的金胶体颗粒的方法,其特征在于,分散有平均粒径在5至100nm范围内的金胶体颗粒(M)的液体和二氧化硅胶体颗粒(A)。 -将平均粒径在4〜40nm的范围内并用含巯基的硅烷化合物进行表面处理并混合了硫醇基(-SH基)的分散液。版权所有:(C)2009,日本特许厅&INPIT

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号