PROBLEM TO BE SOLVED: To provide mixed powder for a sintered Al-containing Cu alloy capable of obtaining a Cu-Al sintered alloy having satisfactory moldability, having high safety upon handling, and dense and having excellent characteristics even at a low sintering temperature of ≤900°C, and to provide a method for producing the same.;SOLUTION: Al-Cu partially dispersed alloyed powder obtained by subjecting mixed powder composed of Al powder of 40 to 60 mass%, and the balance Cu powder is subjected to heating treatment at 540 to 560°C for 10 to 60 min in a reducing or inert atmosphere and pulverizing the same or mixed powder for a sintered Al-containing Cu alloy using Cu-coated Al powder obtained by immersing Al powder into a Cu salt aqueous solution and precipitating 40 to 60 mass% Cu as an Al source is admixed with the three components of 0.05 to 1% P, 0.5 to 4% Si and 0.1 to 1% Sn.;COPYRIGHT: (C)2009,JPO&INPIT
机译:解决的问题:提供一种含铝烧结铜合金的混合粉末,该混合粉末能够获得具有令人满意的成型性,加工时的安全性高,致密且即使在较低的烧结温度下也具有优异的特性的Cu-Al烧结合金。 ; 900℃,并提供一种制备方法。溶液:对铝-铜部分分散的合金粉进行加热处理,该粉通过对由40至60质量%的铝粉组成的混合粉进行热处理,然后对其余的铜粉进行加热在还原性或惰性气氛中在540至560°C下处理10至60分钟,并使用将铝粉浸入铜盐水溶液中而获得的镀铜铝粉将相同或混合的粉末粉碎成含铝的烧结铜合金并沉淀出40至60质量%的铝作为铝源与0.05至1%P,0.5至4%Si和0.1至1%Sn的三种成分混合。;版权:(C)2009,JPO&INPIT

著录项

  • 公开/公告号JP2009007650A

    专利类型

  • 公开/公告日2009-01-15

    原文格式PDF

  • 申请/专利权人 FUKUDA METAL FOIL & POWDER CO LTD;

    申请/专利号JP20070171602

  • 发明设计人 TAKAYA GEN;MASUOKA SACHIKO;

    申请日2007-06-29

  • 分类号B22F1/00;C22C9/01;B22F1/02;

  • 国家 JP

  • 入库时间 2022-08-21 19:43:53

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号