PPROBLEM TO BE SOLVED: To provide a zeolite hydrothermally solidified body having high air permeability and water permeability and excellent function of deodorization and water cleaning. PSOLUTION: The zeolite solidified body is obtained by molding a kneaded material of zeolite powder, an active calcium source and water and subjecting the molded material to water hydrothermally solidification reaction in an autoclave. The quantity of raw material zeolite to be blended is several times to ten times of the quantity of the active calcium source and is set to have 0.1 mm average particle diameter. A part of the raw material zeolite and the active calcium source are reacted with each other to produce calcium silicate hydrate and the raw material zeolite and the active calcium source are solidified by the reaction to secure the strength and to form voids running in all direction. The function such as deodorization is kept because the quantity of zeolite is excessive compared to the quantity of the active calcium source and the high porosity is secured by the large particle diameter of the zeolite. PCOPYRIGHT: (C)2010,JPO&INPIT
机译:

要解决的问题:提供一种具有高透气性和水渗透性以及优异的除臭和水清洗功能的沸石水热固化体。

解决方案:沸石固化体是通过将沸石粉末,活性钙源和水的捏合材料成型,并在高压釜中进行水热固化反应而获得的。混合的原料沸石的量是活性钙源的量的几倍至十倍,并且被设置为具有0.1mm的平均粒径。使一部分原料沸石和活性钙源彼此反应以生成硅酸钙水合物,并且通过该反应使原料沸石和活性钙源固化以确保强度并形成在所有方向上延伸的空隙。由于沸石的量比活性钙源的量过量,并且由于沸石的大粒径确保了高孔隙率,所以保留了除臭等功能。

版权:(C)2010,日本特许厅&INPIT

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号