PROBLEM TO BE SOLVED: To achieve means by which an optically functional layer having optical functions can be imparted regioselectively and spatial selectively to the surface or inside of a fiber coated or mixed with a compound having an Si-O-Si bond.;SOLUTION: The method for producing the smart fiber includes selectively irradiating the fiber 1 coated or mixed with the compound having the Si-O-Si bond with a first light 3 having a wave length or 190 nm or less, a second light 5 having a wave length of less than 190 nm and more than 266 nm, and a third light 6 having a wave length of 266 nm or more to form one of a silica glass layer 2a, a luminescent material layer 2b and a carbon layer 2c of an optically functional layer 2 polyphyletically at the part irradiated with the light.;COPYRIGHT: (C)2009,JPO&INPIT
机译:解决的问题:为了实现一种手段,可以将具有光学功能的光学功能层区域选择性地和空间选择性地赋予涂覆或混合有具有Si-O-Si键的化合物的纤维的表面或内部;解决方案:用于制造智能纤维的方法包括:用波长为190nm以下的第一光3,波长为190nm以下的第一光3选择性地照射涂覆或混合有具有Si-O-Si键的化合物的纤维1。小于190nm且大于266nm的光,以及波长为266nm或更大的第三光6形成光学功能层的石英玻璃层2a,发光材料层2b和碳层2c中的一个光线照射部分多角2。版权所有:(C)2009,JPO&INPIT

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号