The methods for making a coated thin veneer, plank or wood product in which the coated surface does not crack due to instability of the wood involve applying to a veneer, plank or wood product a composition including a hydrophilic polymer and a reactive monomer or a composition including a reactive (meth)acrylate. In one embodiment, the hydrophilic polymer is a polyalkylene glycol, such as polyethylene glycol. The composition also advantageously includes a thermally activated free radical initiator, a photoinitiator or both. The veneer is further laminated into wood product boards that are cut down to planks. In another aspect of the current invention, several solvent based resins are roll coated onto the loose and/or tight side of the thin veneer or unfinished plank wood, dried to remove solvent, and exposed to UV radiation to cure the resinous material by radical initiation of the photoinitiator that leads to polymerization. Further polymerization of the resin material within the pores or voids occurs by heat induced initiation of the organic peroxides at the time of lamination in the case of veneer or by UV radiation exposure in the case of planks.
机译:制备涂覆的薄木皮,木板或木制品的方法,其中涂覆的表面不会由于木材的不稳定性而破裂,该方法包括将包含亲水性聚合物和反应性单体的组合物施涂到木皮,木板或木制品上或该组合物包括反应性(甲基)丙烯酸酯。在一个实施方案中,亲水性聚合物是聚亚烷基二醇,例如聚乙二醇。该组合物还有利地包括热活化的自由基引发剂,光引发剂或两者。将单板进一步层压到切成木板的木制品板上。在本发明的另一方面,将几种基于溶剂的树脂辊涂在薄单板或未加工的木板的松散和/或紧密的一侧上,干燥以除去溶剂,并暴露于紫外线辐射下以通过自由基引发来固化树脂材料。引发聚合反应的光引发剂。如果是单板,则在层压时通过热诱导引发有机过氧化物,或者如果是木板,则通过暴露于紫外线辐射,从而在孔隙或空隙内使树脂材料进一步聚合。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号