LIGHT WOOD-BASED MATERIAL, COMPOSITE MATERIAL, PROCESS FOR THE PRODUCTION OF LIGHT WOOD-BASED MATERIALS, AND USE OF WOOD-BASED MATERIALS

机译:轻木基材料,复合材料,轻木基材料的生产过程以及木基材料的使用

摘要

Light, wood-containing material (I) with an average density of 200-600 kg/m 3, comprises wood particles (a) (30-95 wt.%); fillers (b) (1-25 wt.%) with a bulk density of 10-150 kg/m 3, from foamable plastic particles and plastic particles that are already foamed; binders (c) (0.1-50 wt.%); and optionally additives (d), where (b) contains foaming plastic particles (1-100 wt.%) gained by comminution from molds. Independent claims are included for: (1) a multilayer wood material, comprising at least three layers, where only middle layer or at least one part of the middle layer contains (I), and the external surface layer does not contain fillers; and (2) a preparation of (I) comprising mixing the components (a-d), and subsequently pressing under increased temperature and pressure.
机译:平均密度为200-600 kg / m 3>的轻质含木材料(I),包含木颗粒(a)(30-95 wt。%);从可发泡塑料颗粒和已经发泡的塑料颗粒中填充密度为10-150 kg / m 3>的填料(b)(1-25 wt。%);粘合剂(c)(0.1-50重量%);以及任选地添加剂(d),其中(b)包含通过从模具粉碎得到的发泡塑料颗粒(1-100 wt。%)。包括以下独立权利要求:(1)一种多层木材料,包括至少三层,其中仅中间层或中间层的至少一部分包含(I),并且外表面层不包含填料。 (2)制备(I)的方法,包括混合组分(a-d),然后在升高的温度和压力下压制。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号