The invention relates to a process for the recovery purification of nickel ions from residual solutions. According to the invention, the process consists, in a first stage, in extracting the nickel ion as nickel oxalate dihydrate, under the following optimal reaction conditions: the molar nickel concentration within the residual solution0.02, the solution pH=4.5, excess oxalic acid of 100%, the reaction temperature of 80A C; further on, the nickel oxide is obtained by thermal decomposition of the resulting nickel oxalate, at a temperature of 320...360A C.
机译:本发明涉及从残余溶液中回收纯化镍离子的方法。根据本发明,该方法的第一步是在以下最佳反应条件下提取草酸镍二水合物形式的镍离子:残余溶液中镍的摩尔镍浓度> 0.02,溶液pH = 4.5,过量草酸酸为100%,反应温度为80℃。此外,在320 ... 360A C的温度下,通过热分解生成的草酸镍获得氧化镍。

著录项

  • 公开/公告号RO122090B1

    专利类型

  • 公开/公告日2008-12-30

    原文格式PDF

  • 申请/专利权人 UNIVERSITATEA ORADEA;

    申请/专利号RO20030000309

  • 发明设计人 GAVRI GEORGETA;

    申请日2003-04-10

  • 分类号C02F1/54;C22B23/00;

  • 国家 RO

  • 入库时间 2022-08-21 19:25:48

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号