RAW AND FRITTED MIXTURES FOR GLAZES AND ENAMELS BASED ON KAOLINITE AND BORON MINERALS (HAULITE AND COLEMANITE)

机译:基于高岭石和硼矿物(硅藻土和钙锰矿)的釉料和搪瓷混合物

摘要

The product of row and fritted mixtures for glazes and enamels is based on kaolinite from Pčinj region and borate mineral stones (haulite and colemanite) from Baljevac, on the river of Ibar, it is made completely from domestic mineral raw materials and can definitely substitute expensive imported frittes in all our factors for glazing ceramic and enameling metallic products and also can be exported abroad. Raw and fritted mixtures for glazes have the following approximate composition. Minerological composition: K and Na feldspar 17,7 %, calcite 8,9 %, boron minerals haulite, colemanite 26,4%, kaolinite 47,0 %; and chemical composition: raw SIO2 51,0 % and fritted 57,2 %, raw Al2O3,6 % and 13,0 %, raw CaO 11,2 % and fritted 12,5 %; raw B2O3 11,0 % and fritted 12,3 %, raw K2O 1,3 and fritted 1,4 %; raw Na2O 3,2 % and fritted 3,6 %, while the heating loss is 10,7 %.Raw and fritted mixture for enameling has the following approximate composition. Minerological composition: kaolinite 44,12 %, boron minerals 38,24 %, calcite 8,82 %, K and Na feldspar 8,82 %; and raw chemical composition SiO2 43,0 % and fritted 49,4 %, raw B2O3 16,0 % and fritted 18,4 %, raw CaO 14,0 % and fritted 16,1%, raw Al203 10,0 % and fritted 11,5 %, K2O 2,4 % and fritted 2,8 %, raw Na2O 1,6 % and fritted 1,8 %, and the heating loss is 13,0 %.
机译:釉料和搪瓷的行和烧结混合物的产品是基于Pč in地区的高岭石和Ibar河上Baljevac的硼酸盐矿物石(硅藻土和硬锰矿),完全由国内矿物原料制成,可以在我们所有的因素中,可以代替昂贵的进口玻璃料来给陶瓷和搪瓷金属产品上光,也可以出口到国外。釉料的生料和烧结料混合物具有以下近似组成。矿物学组成:钾和钠长石为17.7%,方解石为8.9%,硼矿物为轻铁矿,硬锰矿为26.4%,高岭石为47.0%;化学成分:原料SIO 2为51.0%,烧结而成的坯料为57.2%,原料Al 2 O 3为6.6%和烧结成坯的13.0%,原料CaO为11.2%,烧结成坯的为12.5%。原料B2O3的含量为11,0%,烧结的为1,2.3%,原料K2O3的含量为1,3%的烧结的;原始Na2O含量为3,2%,烧结的毛坯含量为3.6%,而加热损失为10,7%。用于搪瓷的生料和烧结的混合物具有以下近似组成。矿物学组成:高岭石44,12%,硼矿38,24%,方解石8,82%,钾和钠长石8,82%;化学成分为SiO2 43,0%和烧结的49,4%,原始B2O3为16.0%和烧结的18.4%,原始CaO为14.0%和烧结的16.1%,原始Al2O3为10,0%的烧结的11.5%,K 2 O 2.4%和烧结的2.8%,粗Na 2 O 1.6%和烧结的1.8%,加热损失为13.0%。

著录项

  • 公开/公告号RS20070322A

    专利类型

  • 公开/公告日2008-11-28

    原文格式PDF

  • 申请/专利权人 JOVANOVIC TOMISLAV;

    申请/专利号RS2007P000322

  • 发明设计人 JOVANOVIC TOMISLAV;

    申请日2007-07-30

  • 分类号C03C8/00;

  • 国家 RS

  • 入库时间 2022-08-21 19:25:46