首页> 外国专利> Aromatic polymers of rubber modified high gloss produced by a process of bulk polymerization movilinilideno.

Aromatic polymers of rubber modified high gloss produced by a process of bulk polymerization movilinilideno.

机译:橡胶改性的高光泽度的芳香族聚合物,是通过本体聚合莫维尼利诺德工艺生产的。

摘要

A polymer composition modified mass polymerized rubber comprising: a continuous matrix phase comprising a polymer of a monovinylidene aromatic monomer and optionally a monomer ethylenically unsaturated nitrile, and discrete rubber particles dispersed in said matrix, produced said particles rubber from a rubber component comprising from 5 to 100 weight percent of a functionalized diene rubber having at least one functional group per rubber molecule capable of enabling controlled radical polymerization; wherein the composition is further characterized by: a) an average size of rubber particle volume from about 0.15 to 0.35 micron, b) a total rubber phase volume between 12 and 45 percent, based on the volume total combination of the matrix phase and the rubber particles; c) a partial rubber phase volume between 2 and 20 percent characterized by rubber particles having an average particle size greater than 0.40 micrometers by volume; and d) a crosslinked rubber fraction of at least 85 weight percent, based on the total weight of the rubber particles; It is the ad parameters measured by the methods described in the description.
机译:聚合物组合物改性的本体聚合橡胶,其包含:连续的基体相,所述基体包含单亚乙烯基芳族单体和任选的单体烯键式不饱和腈的聚合物,以及分散在所述基体中的离散的橡胶颗粒,由包含5至5的橡胶组分制备所述颗粒橡胶100重量%的官能化二烯橡胶,其每个橡胶分子具有至少一个能够进行受控自由基聚合的官能团;其中所述组合物的特征还在于:a)橡胶颗粒体积的平均尺寸为约0.15至0.35微米,b)基于基质相和橡胶的总体积组合,橡胶相的总体积为12至45%粒子; c)部分橡胶相体积在2%至20%之间,其特征在于橡胶颗粒的平均粒径大于0.40体积微米; d)基于橡胶颗粒的总重量,至少85重量%的交联橡胶分数;它是通过说明中描述的方法衡量的广告参数。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号