A process for thermally polymerizing a liquid hydrocarbon pitch precursor, or fractionating a crude pitch, by direct contact heating with an immiscible molten fluid, preferably molten metal, is disclosed. A crude pitch, which may contain water, contaminants and/or distillables, or a liquid hydrocarbon feed such as FCC slurry oil, is heated by direct contact heat exchange with molten fluid, preferably a molten metal bath, operating at a temperature of 100 to 6000C. The bath is maintained at a temperature and pressure sufficient to induce thermal polymerization of a pitch precursor and/or vaporize a desired amount of contaminants or volatile material from a crude pitch to produce a pitch product having a desired softening point. New pitch compositions having a high softening point are also produced.
机译:公开了通过与不混溶的熔融流体,优选熔融金属直接接触加热而使液态烃沥青前体热聚合或分馏粗沥青的方法。粗沥青可以与水(温度范围为100至200℃)操作,通过与熔融流体(最好是熔融金属浴)直接接触换热,从而加热可能含有水,污染物和/或蒸馏物或液态烃原料(例如FCC浆料油)的沥青。 6000摄氏度将该浴保持在足以引起沥青前体的热聚合和/或从粗沥青中汽化所需量的污染物或挥发性物质以产生具有所需软化点的沥青产品的温度和压力。还生产了具有高软化点的新型沥青组合物。

著录项

  • 公开/公告号WO2009074837A1

    专利类型

  • 公开/公告日2009-06-18

    原文格式PDF

  • 申请/专利权人 DTX TECHNOLOGIES LLC;MALONE DONALD P.;

    申请/专利号WO2007IB03836

  • 发明设计人 MALONE DONALD P.;

    申请日2007-12-10

  • 分类号C10G9/00;C10C1/19;C10C3/00;

  • 国家 WO

  • 入库时间 2022-08-21 19:18:17

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号