Disclosed are a method for producing wide flat steel by thin slab continuous casting and rolling and the system thereof. The method includes the following steps: the molten steel is first continuously cast into a thin slab of 50~90mm thickness; then the thin slab is carried out even heating, electromagnetic induction heating, surface descaling, hot strip rolling, laminar flow cooling and coiling. Through regulating the technological parameters of the method, the solid solution and precipitation behaviors of carbon, nitrogen and sulfide in steel are controlled, and finally, qualified wide flat steel can be obtained. The system mainly consist of a slab continuous caster, a slab shearing equipment, a roller-hearth furnace, a slab electromagnetic induction heating stove, a high-pressure water descaling device, a hot strip mill, a laminar flow cooling device and a steel strip coiling apparatus which are successively connected. The slab electromagnetic induction heating stove is comprised of a quick electromagnetic induction zone and an electromagnetic induction holding zone. The method and the system can effectively control the solid solution and precipitation behaviors of carbon, nitrogen and sulfide in steel, and produce high quality of broad hot strips with lower cost and by more flexible process.
机译:本发明公开了一种通过薄板坯连铸轧制生产宽扁钢的方法及其系统。该方法包括以下步骤:首先将钢水连续铸造成厚度为50〜90mm的薄板坯;然后对薄板坯进行均匀加热,电磁感应加热,表面除氧化皮,热轧带钢,层流冷却和卷取。通过调节该方法的工艺参数,可以控制钢中碳,氮和硫化物的固溶体和析出行为,最后可以得到合格的宽扁钢。该系统主要由板坯连铸机,板坯剪切设备,辊底式炉,板坯电磁感应加热炉,高压水除鳞装置,热轧机,层流冷却装置和钢带组成依次连接的卷取装置。平板电磁感应加热炉由快速电磁感应区和电磁感应保持区组成。该方法和系统可以有效地控制钢中碳,氮和硫化物的固溶和析出行为,并以较低的成本和更灵活的工艺生产出高质量的宽幅热轧带钢。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号