method for producing a thermoplastic resin prepreg and the thermoplastic resin prepreg manufactured by that method are disclosed. The manufacturing method of the disclosed thermoplastic resin prepreg, (a) providing a substrate, (b) a step of impregnating the first thermoplastic resin composition solution to the substrate, (c) the substrate is impregnated in the composition solution is 2 including the step of impregnating a thermoplastic resin composition solution, and a number average molecular weight of the first thermoplastic resin is smaller than the number average molecular weight of the second thermoplastic resin. ; Thus, the disclosed thermoplastic method for producing a resin prepreg is not only the impregnation improved emulsifier, a plasticizer, or a viscosity reducing agent is not necessary and the cost of the product can be reduced by simplifying the process. Further, the thermoplastic resin prepreg prepared by the above method, he does not include a low molecular weight substance.
机译:公开了一种热塑性树脂预浸料的制造方法以及通过该方法制造的热塑性树脂预浸料。所公开的热塑性树脂预浸料的制造方法,(a)提供基材,(b)将第一热塑性树脂组合物溶液浸渍到基材上的步骤,(c)将基材浸渍在组合物溶液中的步骤包括:通过使热塑性树脂组合物溶液浸渍,可以使第一热塑性树脂的数均分子量小于第二热塑性树脂的数均分子量。 ;因此,所公开的用于生产树脂预浸料的热塑性方法不仅不需要浸渍改进的乳化剂,增塑剂或粘度降低剂,而且可以通过简化工艺来降低产品成本。此外,通过上述方法制备的热塑性树脂预浸料不包含低分子量物质。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号