A method for manufacturing liquid mortar using raw loess is provided to exhibit excellent intensity and adhesive force without the use of cement and to facilitate a process of mixing with additional water. A method for manufacturing liquid mortar using raw loess comprises the following steps of: mixing quicklime, ferrous sulfate heptahydrate anhydride and raw loess(S1); curing the mixture to stabilize its moisture and reaction heat(S2); removing foreign materials from the mixture(S3); pulverizing the mixture to prepare loess powder(S4); mixing stone flour and the mixture to prepare a solid portion(S5); mixing water and polyvinyl alcohol and dissolving to prepare a polyvinyl alcohol solution(S6); mixing water and a polymer coagulant and dissolving to prepare a polymer coagulant solution(S7); mixing the polyvinyl alcohol solution and the polymer coagulant solution in a certain ratio to obtain a liquid binder(S8); and mixing the solid portion and the liquid binder to obtain the liquid mortar(S9).
机译:本发明提供一种使用生黄土的液态砂浆的制造方法,该方法在不使用水泥的情况下显示出优异的强度和粘合力,并且有助于与额外的水混合的过程。一种利用生黄土生产液态砂浆的方法,包括以下步骤:将生石灰,七水合硫酸亚铁和生黄土混合(S1);使混合物固化以稳定其水分和反应热(S2);从混合物中去除异物(S3);将混合物粉碎以制备黄土粉(S4);将石粉和混合物混合以制备固体部分(S5);将水和聚乙烯醇混合并溶解以制备聚乙烯醇溶液(S6);将水和聚合物凝结剂混合并溶解以制备聚合物凝结剂溶液(S7);将聚乙烯醇溶液和聚合物凝结剂溶液以一定比例混合以获得液体粘合剂(S8)。将固体部分和液体粘合剂混合以获得液体砂浆(S9)。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号