首页> 外国专利> Procedure for the production of stone grain and stone grain, in particular for building materials

Procedure for the production of stone grain and stone grain, in particular for building materials

机译:石粒和石粒,特别是建筑材料的生产程序

摘要

Process for production of variable grain size stone composition for building materials, e.g. concrete, especially a light admixture composition, involving:(a) preparation of a homogeneous starting mixture from:(weight %):cement (1-10), fired clay (20-85), burnt plant ash (10-40), flue dust (0-35), light admixture (0-1) and water, where the ratio of the weight of water to the total dry weight of starting mixture = 0.20-0.35, (b) preparation of a molded article from the starting mixture, and (c) setting (sic) of the molded article at a temperature of 80 deg.C, where the molded article is hardened to particles of variable grain size stone composition. An independent claim is included for a variable grain size stone composition.
机译:生产用于建筑材料的可变粒度石材组合物的方法,例如混凝土,尤其是轻质掺合料组合物,涉及:(a)由以下物质制备均质的起始混合物:(重量%):水泥(1-10),烧成粘土(20-85),烧成植物灰(10-40),烟道粉尘(0-35),轻质混合物(0-1)和水,其中水的重量与原料混合物的总干重之比= 0.20-0.35,(b)从原料制备模制品(c)在80℃的温度下将模塑制品凝固(sic),在此温度下模塑制品被硬化成具有可变粒度的石材组成的颗粒。对于可变粒度的石材组成,还包括独立权利要求。

著录项

  • 公开/公告号DE502007001139D1

    专利类型

  • 公开/公告日2009-09-03

    原文格式PDF

  • 申请/专利权人 LIAPOR GMBH & CO. KG;

    申请/专利号DE20075001139T

  • 发明设计人 FUCHS WOLFGANG;HENNEK PAUL;

    申请日2007-05-21

  • 分类号C04B18/02;

  • 国家 DE

  • 入库时间 2022-08-21 19:08:38

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号