PROBLEM TO BE SOLVED: To provide a method of preparing an iron-oxide adsorbent suitable for isolating an oxyacid ion of molybdenum contained in acidic waste water of pH2 or lower, and a method of cleaning molybdenum-containing waste water suitable for isolating an oxyacid ion of molybdenum from acidic waste water of pH2 or lower using the adsorbent.;SOLUTION: The method of preparing an iron-oxide adsorbent is characterized by adding an alkali into a solution comprising ferric ions and mixing them for neutralizing the solution to form a precipitate, drying the resulting precipitate at a temperature of 60 to 100°C to obtain a ferric hydroxide powder, and further calcining the resulting ferric hydroxide powder at a temperature of 300 to 700°C. The method of cleaning molybdenum-containing waste water comprises treating molybdenum-containing waste water by allowing it to flow through a column filled with the adsorbent and isolating molybdenum anions from the molybdenum-containing waste water.;COPYRIGHT: (C)2010,JPO&INPIT
机译:解决的问题:提供一种制备适于分离pH 2以下的酸性废水中所含的钼的含氧离子的氧化铁吸附剂的方法,以及一种适于分离含氧离子的含钼废水的清洁方法。解决方案:制备铁氧化物吸附剂的方法的特征在于,将碱添加到含铁离子的溶液中并混合以中和该溶液以形成沉淀,在60至100℃的温度下干燥所得沉淀物以获得氢氧化铁粉末,并在300至700℃的温度下进一步煅烧所得的氢氧化铁粉末。清洁含钼废水的方法包括通过使含钼废水流经装有吸附剂的色谱柱并从含钼废水中分离出钼阴离子来对其进行处理。版权所有(C)2010,JPO&INPIT

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号