PPROBLEM TO BE SOLVED: To provide a hydraulic slag processing method for a wrought steel furnace capable of preventing pollution with hydraulic power and recycling slag. PSOLUTION: Slag is sent to a hydraulic sorting device through a raw material hopper, and sorted to four groups of slag of 30 mm or more, 12-30 mm, 8-12 mm and 8 mm or less. Residual steel containing iron is separated from the slag by a magnetic selector, and the slag of 30 mm or more is crushed by a crusher. The residual steel containing iron is separated by the magnetic selector, and the left slag is sent to a grinder for grinding through a secondary raw material hopper, and thereafter, returned to the raw material hopper and processed again. A water sprinkler is provided inside the hydraulic sorting device, and the slag at 8 mm or less is eliminated by filtering sand contained in the slag by the hydraulic machine, and the water, from which sand is eliminated by filtration, is sent into a settling tank, and lime powder is settled, and the water is circulated to the sprinkler device for recycle. PCOPYRIGHT: (C)2006,JPO&NCIPI
机译:

要解决的问题:提供一种用于锻钢炉的水渣处理方法,该方法能够防止水力动力污染和回收渣。

解决方案:炉渣通过原料料斗送入液压分选设备,然后分选为30毫米或更大,12-30毫米,8-12毫米和8毫米或更小的四组炉渣。残留的含铁钢通过磁力选择器从炉渣中分离出来,并用破碎机将30 mm以上的炉渣破碎。含铁的残留钢被磁性选择器分离,残留的炉渣通过第二个原料料斗送入研磨机进行研磨,然后返回原料料斗并再次加工。在水力分选装置的内部设置有洒水装置,通过液压机对渣中所含的砂进行过滤,从而将8mm以下的炉渣除去,将通过过滤除去了砂的水送入沉降池。在水箱中沉淀石灰粉,然后将水循环到洒水装置中进行回收。

版权:(C)2006,JPO&NCIPI

著录项

  • 公开/公告号JP4559762B2

    专利类型

  • 公开/公告日2010-10-13

    原文格式PDF

  • 申请/专利权人 鄭志強;鄭至佑;鄭志誠;

    申请/专利号JP20040092338

  • 发明设计人 鄭志強;鄭至佑;鄭志誠;

    申请日2004-03-26

  • 分类号C04B5;B03B7;

  • 国家 JP

  • 入库时间 2022-08-21 19:02:48

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号