首页> 外国专利> In order production manner of the crystal Characteristic tobamoraito high content die concrete and the mixing material null hydraulic property cement for crystal Characteristic tobamoraito high

In order production manner of the crystal Characteristic tobamoraito high content die concrete and the mixing material null hydraulic property cement for crystal Characteristic tobamoraito high

机译:为了生产结晶性高的陶巴莫来托高模量混凝土和掺和料的水硬性结晶特性的水泥

摘要

PROBLEM TO BE SOLVED: To produce concrete containing crystalline tobermorite in a high content, which contributes to heat resistance, by effectively using fly ash.;SOLUTION: The concrete containing a large amount of crystalline tobermorite is obtained by mixing 48 parts by mass of portland cement, 8.4 parts by mass of slaked lime, 3.6 parts by mass of gypsum, 40 parts by mass of fly ash, 100 parts by mass of quartz sand No. 5 as aggregate, and 43 parts by mass of water, then mixing and kneading the resulting mixture, and subjecting the kneaded material to steam autoclave curing at a curing temperature of ≥180°C.;COPYRIGHT: (C)2006,JPO&NCIPI
机译:解决的问题:通过有效地使用粉煤灰,生产高含量的结晶性蒙脱石的混凝土,有助于耐热性;解决方案:混合48质量份的硅酸盐得到大量的结晶性蒙脱石。水泥,熟石灰8.4质量份,石膏3.6质量份,粉煤灰40质量份,5号石英砂100质量份,水43质量份混合搅拌所得混合物,并将捏合后的物料在180℃的固化温度下进行蒸汽高压釜固化。版权所有:(C)2006,JPO&NCIPI

著录项

  • 公开/公告号JP4462538B2

    专利类型

  • 公开/公告日2010-05-12

    原文格式PDF

  • 申请/专利权人 財団法人電力中央研究所;

    申请/专利号JP20040149722

  • 发明设计人 山本 武志;

    申请日2004-05-19

  • 分类号C04B28/18;C04B40/02;

  • 国家 JP

  • 入库时间 2022-08-21 19:00:56

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号