首页> 外国专利> Method for producing a low-sulfur catalytic cracking gasoline desulfurization using the additional function fluid catalytic cracking catalyst method of manufacturing the same, and desulfurization function adds fluid catalytic cracking catalyst

Method for producing a low-sulfur catalytic cracking gasoline desulfurization using the additional function fluid catalytic cracking catalyst method of manufacturing the same, and desulfurization function adds fluid catalytic cracking catalyst

机译:利用附加功能的流化催化裂化催化剂制造低硫催化裂化汽油的方法及其制造方法,以及具有脱硫功能的流化催化裂化催化剂的添加方法

摘要

In the process of producing the catalytic cracking gasoline by decomposition of heavy oil can be efficiently reduced the sulfur content of the catalytically cracked gasoline, and porous inorganic (b) zeolite and non-zeolite was (a) alumina-coated The content and (b) alumina 30 to 70 wt% and 5 to 40 wt% zeolite was coated with (a) alumina or is a catalyst formed by supporting a vanadium carrier comprising a clay mineral and / or oxides It will carry a vanadium carrier which is supported phosphorus and manganese and / or vanadium at least a carrier containing a porous inorganic oxide the ratio of vanadium concentration of before and after grinding, or the two or more catalysts phosphorus to form a complex ion and manganese and / or vanadium in carrying solution when it becomes Te, carrying the phosphorus and manganese and / or vanadium, transmission of the reverse osmosis membrane of the complex ion, the reverse osmosis membrane of vanadium and to provide a catalyst is 25 wt% or less of the amount of transmitted.
机译:在通过重油分解生产催化裂化汽油的过程中,可以有效地降低催化裂化汽油的硫含量,并且多孔无机(b)沸石和非沸石是(a)氧化铝涂层的含量和(b )用(a)氧化铝涂覆30至70 wt%的氧化铝和5至40 wt%的氧化铝,或者是通过负载包含粘土矿物和/或氧化物的钒载体而形成的催化剂。它将承载负载有磷和锰和/或钒中至少一种含有多孔无机氧化物的载体,其研磨前后的钒浓度比,或两种或多种催化剂磷在变成Te时在承载液中形成络合离子和锰和/或钒载有磷,锰和/或钒,络合物离子的反渗透膜,钒的反渗透膜的透射率和提供催化剂的重量百分比小于或等于25%传输量。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号