A process of obtaining silicon nitride (Si3N4) surface coatings on ceramic pieces and components by impregnation of the surfaces of the ceramic pieces with silicon powder suspensions with a particle size preferably less than 200 μm. The thickness of the coatings depends on the impregnation time and on the properties of the slip and the ceramic piece. The subsequent nitridation of the coating by thermal treatment at temperatures between 1300° C. and 1500° C. in N2 atmospheres leads to a continuous Si3N4 coating. The chemical stability and compatibility between Si3N4 and molten silicon enables its application in silicon metallurgy, in manufacturing crucibles for silicon fusion or for housing said molten silicon, in manufacturing pipes and chutes for its transport or in manufacturing different components for its subsequent purification.
机译:一种通过用粒径大小的硅粉悬浮液浸渍陶瓷片表面来在陶瓷片和组件上获得氮化硅(Si 3 N 4 )表面涂层的方法优选小于200μm。涂层的厚度取决于浸渍时间以及泥浆和陶瓷片的性能。随后在N 2 气氛中于1300°C至1500°C的温度下通过热处理对涂层进行氮化,从而导致连续的Si 3 N 4 涂层。 Si 3 N 4 与熔融硅之间的化学稳定性和相容性使其可用于硅冶金,制造用于熔融硅的坩埚或用于容纳所述熔融硅的制造管道中溜槽用于运输或制造用于后续纯化的不同组件。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号