The present invention refers to a method and an equipment for curing and drying self-reducing agglomerates containing cement as a binder in the presence of saturated vapor at a temperature from about 70 to about 110° C. and under atmospheric pressure. The treatment is performed in one single equipment. The self-reducing agglomerates are comprised of mixtures of fines of iron ore and/or industrial residue containing iron oxides and/or metallic iron, fines of carbonaceous materials such as mineral coal, charcoal, green petroleum coke and similar fines, fluxing material such as steel plant slag and blast furnace slag, limestone, lime and similar materials, cement as a binder and fluxing agent, and humidity between 7 and 12%, produced in pellet-making units and/or briquette-making units and thereafter treated using one single piece of equipment, involving the steps of predrying with heated gasses (2), curing with saturated vapor (3) and drying with heated gasses (4) performed continuously and sequentially, controlling the discharge velocity (5) in order to allow the time of permanence of the agglomerate within the equipment to be from about 4 to about 12 hours. The cured and dried agglomerate may be processed in an adequate reducing/melting equipment to provide metals and metallic alloys.
机译:本发明涉及在约70至约110℃的温度和大气压下在饱和蒸气存在下固化和干燥包含水泥作为粘合剂的自还原性附聚物的方法和设备。该处理在一台设备中进行。自还原性附聚物由铁矿石细粉和/或含有氧化铁和/或金属铁的工业残渣的混合物,含碳物质如矿物煤,木炭,绿色石油焦和类似的细粒的混合物,助熔材料如以下混合物组成:钢铁厂矿渣和高炉矿渣,石灰石,石灰和类似材料,作为粘结剂和助熔剂的水泥,湿度在7%至12%之间,在制粒机和/或压块机中生产,然后使用一个单一装置进行处理该设备连续连续地进行以下步骤:用加热气体预干燥(2),用饱和蒸汽固化(3)和用加热气体干燥(4),并控制排出速度(5),以确保排出时间设备内附聚物的持久性为约4至约12小时。可以在足够的还原/熔化设备中处理固化和干燥的团聚物,以提供金属和金属合金。

著录项

  • 公开/公告号BR0208171B1

    专利类型

  • 公开/公告日2010-08-10

    原文格式PDF

  • 申请/专利权人

    申请/专利号BR20020208171

  • 申请日2002-03-19

  • 分类号C22B1;C22B1/243;C22B1/24;C22B1/245;F27B1;F27B1/02;F27B1/26;F27D7/02;

  • 国家 BR

  • 入库时间 2022-08-21 18:47:27

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号