a method for superconducting connection of two or more wires (1, 2), each of which at least one filament (3a - 3d) in which mgb2 or containing a mixture of mg and b containswith the superconducting connection exposed endbereiche (4a) of the filaments (3a - 3d) on a mgb2 matrix is characterized by the fact that(a) a pulverschu00fcttung (4) of boron powder is provided, in which the exposed endbereiche (4a) of the filaments (3a to 3d) of the wires (1, 2) hineinragen, while the boron of the boron powder, the pulverschu00fcttung (4) in amorphous modification.(b) the pulverschu00fcttung (4) with the hineinragenden, exposed endbereiche (4a) of the filaments (3a, 3b) to an extruded elements (8) is compressed.(c) and the extruded elements (8) from the surface (13) of the pressku00f6rpers (8) of a magnesium melt (10) infiltrated. with the erfindungsgemu00e4u00dfen procedure, the quality, especially the stromtragfu00e4higkeit and critical necessary, a superconducting connection of mgb2 - supraleiterdru00e4hten are improved.
机译:一种超导连接两根或多根电线(1、2)的方法,每根电线至少有一根灯丝(3a-3d),其中mgb2或含有mg和b的混合物具有超导连接的mgb2基质上的细丝(3a-3d)的暴露的endereiche(4a)具有以下特征:(a)提供粉末状的硼粉(4),其中,金属丝(1、2)的细丝(3a至3d)的丝线(3a至3d)的裸露末端(4a),而硼粉中的硼,无定形修饰的粉末(4)。(b)将粉末(4)与hineinragenden混合,将长丝(3a,3b)的裸露的小生菌(4a)暴露在挤出元件(8)上。(c)和从镁熔体(10)的压力(8)的表面(13)渗入的挤压元件(8)渗入。通过erfindungsgem的质量,尤其是stromtragf的质量和至关重要的必要条件,mgb2-supraleiterdr u00e4hten的超导连接得以改善。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号