首页> 外国专利> MANUFACTURING METHOD OF SEALING GLASS FOR INTERMEDIATE TEMPERATURE PLANAR SOFC

MANUFACTURING METHOD OF SEALING GLASS FOR INTERMEDIATE TEMPERATURE PLANAR SOFC

机译:中温平面SOFC密封玻璃的制造方法

摘要

PURPOSE: A method for manufacturing sealing glass for flat solid oxide fuel cell of middle low temperature is provided to effectively perform sealing without mixing fuel gas and air. CONSTITUTION: A composition of sealing glass for flat solid oxide fuel cell contains 100 weight parts of glass having 35-45 weight% of BaO, 25-35 weight% of SiO, 10-20 weight% of B2O3, 8-15 weight% of Al2O3; 1-5 weight% of metal oxide selected from CeO2, Fe2O3, Mn2O3 and Cr2O3.
机译:目的:提供一种用于制造中低温扁平固体氧化物燃料电池的密封玻璃的方法,以在不混合燃料气体和空气的情况下有效地进行密封。组成:用于扁平固体氧化物燃料电池的密封玻璃组合物包含100重量份的玻璃,该玻璃具有35-45重量%的BaO,25-35重量%的SiO,10-20重量%的B2O3、8-15重量%的玻璃。 Al2O3; 1-5重量%的选自CeO 2,Fe 2 O 3,Mn 2 O 3和Cr 2 O 3的金属氧化物。

著录项

  • 公开/公告号KR20100008264A

    专利类型

  • 公开/公告日2010-01-25

    原文格式PDF

  • 申请/专利权人 HYUNDAI MOTOR COMPANY;

    申请/专利号KR20080068747

  • 发明设计人 KIM BYONG SOO;

    申请日2008-07-15

  • 分类号C03C3/062;C03C3/064;

  • 国家 KR

  • 入库时间 2022-08-21 18:33:29