MESOPOROUS PALLADIUM-ALUMINA CATALYST FOR MILD HYDROCRACKING, PREPARATION METHOD THEREOF, AND METHOD FOR PRODUCING MIDDLE DISTILLATE THROUGH HYBRID FISCHER-TROPSCH SYNTHESIS USING SAID CATALYST

机译:用于轻度加氢的介孔钯铝催化剂,其制备方法,以及利用所述催化剂通过混合费-托合成生产中等馏出液的方法

摘要

PURPOSE: A porous palladium-alumina catalyst for hybrid Fischer - Tropsch synthesis, a manufacturing method thereof, a continuous flow double reaction device, and a manufacturing method of middle distillate using the same are provided to increase dispersion of palladium compared to the other catalyst. CONSTITUTION: A manufacturing method of a porous palladium - alumina catalyst for hybrid Fischer - Tropsch synthesis includes the following steps: manufacturing an aluminum - palladium precursor mixed solution by mixing palladium precursor alcohol in a mixed solution of an aluminum precursor alcohol solution and an anionic micelle alcohol solution; manufacturing slurry by maintaining a temperature of the aluminum - palladium precursor mixed solution at 80 ~ 120 C; drying and washing the aluminum - palladium precursor mixed solution; and sintering the dried aluminum palladium precursor slurry at a temperature of 500 ~ 1000 C.
机译:用途:提供用于混合费-托合成的多孔钯-氧化铝催化剂,其制造方法,连续流双反应装置以及使用该催化剂的中间馏分的制造方法,以与其他催化剂相比增加钯的分散性。组成:费-托混合杂化的多孔钯-氧化铝催化剂的制造方法包括以下步骤:通过将钯前体醇在铝前体醇溶液和阴离子胶束的混合溶液中混合来制造铝-钯前体混合溶液。酒精溶液通过将铝-钯前体混合溶液的温度保持在80〜120℃来制造浆料。干燥并洗涤铝-钯前驱体混合溶液;并在500〜1000℃的温度下烧结干燥的铝钯前驱体浆料。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号