FIELD: jewellery production.;SUBSTANCE: invention may be used for soldering of jewellery chains from alloys of 14 carat gold, mostly of red and green colours, and alloys of 18 carat gold. Prior to soldering chains are soaked in blocking solution, which contains trichloroethylene or 1-bromine-propane or dichloromethane as dissolvent, and colophony as dissolved substance. Concentration of solution for chains with wire diametre from 0.2 mm to 0.5 mm inclusive makes 20±4 g/l, and for chains with wire diametre from 0.5 mm to 1.5 mm - 40±4 g/l. Then chains are dried and treated with adhesive-insulating mixture, which contains the following components, wt %: talc powder - 75, castor oil - 23, Vaseline - 1 and lanoline - 1. Soldering is executed in belt electric resistance furnaces in restorative gas atmosphere, containing mixture H2:N2=3:1.;EFFECT: method provides for simplification and acceleration of technological cycle of soldering and makes it possible to completely reject use of ignoble powders of solder.;1 ex
机译:领域:珠宝生产。物质:本发明可用于焊接由14克拉金(主要为红色和绿色)的合金以及18克拉金的合金制成的珠宝链。焊接之前,将链条浸入封闭溶液中,该封闭溶液包含三氯乙烯或1-溴丙烷或二氯甲烷作为溶剂,而树脂为溶解物质。对于线径为0.2 mm至0.5 mm(含端值)的链,溶液的浓度为20±4 g / l,对于线径为0.5 mm至1.5 mm的链则为40±4 g / l。然后将链条干燥并用绝缘粘合剂混合物处理,该混合物包含以下成分,按重量百分比计:滑石粉-75,蓖麻油-23,凡士林-1和羊毛脂-1。在带电阻炉中在还原性气体中进行焊接气氛,包含混合物H 2 :N 2 = 3:1 。;效果:该方法可简化并加速焊接工艺周期,并有可能完全拒绝使用易碎的焊料粉末。; 1 ex

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号