PROBLEM TO BE SOLVED: To provide a β type titanium alloy having high strength, requires no expensive additional elements, thus, low in cost, but enabling easy mass-production of a component, and to provide a method of producing a component having high strength using the alloy as the material.;SOLUTION: The β type titanium alloy has an alloy composition comprising, by mass, 10 to 20% Cr and ≤5% Fe, and the balance Ti with inevitable impurities. Further, either or both of ≤7% Ni and ≤6% Al can be incorporated therein. In one method for producing the component, the β type titanium alloy is forged or rolled at β transus or higher and also at ≤1,100°C into a component, and the component is successively subjected to solution heat treatment to recrystallize crystal grains. Preferably, aging treatment is further performed. In an another method, the β type titanium alloy is cold-worked successively to the forging or rolling so as to be a component. Preferably, solution heat treatment is performed prior to the cold working. Further, aging treatment is preferably performed after the cold working.;COPYRIGHT: (C)2005,JPO&NCIPI
机译:要解决的问题:提供β具有高强度的钛型钛合金,不需要昂贵的附加元素,因此,成本低,但易于批量生产零件,并提供一种使用合金作为材料生产具有高强度零件的方法。 :β钛合金的合金组成按质量计包括10%至20%的Cr和≤5%的Fe以及余量的Ti和不可避免的杂质。此外,可以在其中掺入≤7%的Ni和≤6%的Al中的任一个或两者。在一种生产该组分的方法中,β是β。型钛合金是在β在高于或等于1100℃的温度下转变成组分,然后对该组分进行固溶热处理以使晶粒重结晶。优选地,进一步进行时效处理。在另一种方法中,β型钛合金是在锻造或轧制过程中先后进行冷加工而制成的。优选地,在冷加工之前进行固溶热处理。此外,优选在冷加工之后进行时效处理。;版权所有:(C)2005,JPO&NCIPI

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号