PROBLEM TO BE SOLVED: To develop a glaze for a Kimachi-like ceramic, a Kimachi-like ceramic product, and a method for producing the product.;SOLUTION: The glaze for the Kimachi-like ceramic contains, in Seger expression, 0 to 0.6 mol of CaO, 0 to 0.5 mol of MgO, 0 to 0.5 mol of ZnO, 0.5-1.5 mol of Al2O3, 0.2-0.6 mol of P2O5, and 1.0-3.0 mol of SiO2. The Kimachi-like ceramic product (roof tile) is obtained by applying the glaze, and the method for producing the product comprises firing a glazed body at a temperature of ≤1,250°C.;COPYRIGHT: (C)2008,JPO&INPIT
展开▼
机译:要解决的问题:开发用于类似Kimachi的陶瓷的釉料,一种类似Kimachi的陶瓷产品及其生产方法;解决方案:用于类似Kimachi的陶瓷的釉以Seger表示包含> 0到0.6摩尔的CaO,> 0到0.5摩尔的MgO,> 0到0.5摩尔的ZnO,0.5-1.5摩尔的Al 2 Sub> O 3 Sub>,0.2-0.6摩尔P 2 Sub> O 5 Sub>和1.0-3.0 mol SiO 2 Sub>。通过涂覆釉获得类似Kimachi的陶瓷产品(屋面瓦),并且该产品的生产方法包括在1,250℃的温度下烧制釉体;版权所有:(C)2008,JPO&INPIT