首页> 外国专利> The frother for the plasticity lightweight injection material and production manner and that restoration construction method null hydrocarbon type surface active agent of the plasticity lightweight

The frother for the plasticity lightweight injection material and production manner and that restoration construction method null hydrocarbon type surface active agent of the plasticity lightweight

机译:用于可塑性轻质注射剂的发泡剂和生产方式以及修复施工方法可塑性轻质的废烃型表面活性剂

摘要

PPROBLEM TO BE SOLVED: To provide a foaming agent for a plasticized lightweight grouting material, having a light weight and excellent durability, capable of being gelatinized in an instant, hardly affected by underground water or flowing water, and facilitating limited injection and placing of concrete in water; and to provide the plasticized lightweight grouting material using the foaming agent, a production method thereof, and a grouting method thereof. PSOLUTION: The foaming agent for the plasticized lightweight grouting material is obtained by using a hydrocarbon-based surfactant and/or a protein-based surfactant as a main component, and formulating a clayey mineral therewith. The plasticized lightweight grouting material is obtained by mixing foam foamed by the foaming agent with a hardenable liquid containing cement and water for kneading. The proportion of the mixed foam is 15-85% based on the volume of the plasticized lightweight grouting material, and preferably, the flow value and the density of the grouting material are 80-150 mm and 0.3-1.2 g/cmSP3/SPrespectively. The hardenenable liquid and the foam are separately prepared, and the mixing and stirring of both are carried out at the injection site so that the instantly gelatinized injecting material is charged to the injection site, and hardened. PCOPYRIGHT: (C)2004,JPO
机译:

要解决的问题:提供一种用于增塑的轻质灌浆材料的发泡剂,该发泡剂重量轻且具有出色的耐用性,能够瞬间胶化,几乎不受地下水或流水的影响,并且有助于有限的注浆和注水。将混凝土放入水中;并提供使用所述发泡剂的增塑的轻质灌浆材料,其生产方法及其灌浆方法。

解决方案:用于增塑的轻质灌浆材料的发泡剂是通过使用烃基表面活性剂和/或蛋白质基表面活性剂作为主要成分,并由此配制粘土矿物而获得的。通过将由发泡剂发泡的泡沫与包含水泥和水的可硬化液体混合以进行捏合而获得增塑的轻质灌浆材料。基于增塑的轻质灌浆材料的体积,混合泡沫的比例为15-85%,并且优选地,灌浆材料的流量值和密度为80-150mm和0.3-1.2g / cm 2 SP。 3 。分别制备可硬化的液体和泡沫,并且在注射部位进行两者的混合和搅拌,以使即时糊化的注射材料填充到注射部位并硬化。

版权:(C)2004,日本特许厅