PROBLEM TO BE SOLVED: To provide a catalyst which can produce ethylene oxide with high activity and selectivity and to provide a production method of ethylene oxide by gas-phase oxidation of ethylene by a gas containing a molecular oxygen employing the same catalyst.;SOLUTION: The catalyst for producing ethylene oxide is obtained by making a carrier support as a main component of α-Al2O3, wherein an intensity of the infrared adsorption spectrum in the range of wave number of 3,150 to 3,800 cm-1 is substantially zero in the infrared adsorption spectrum measured by the KBr tablet method. The production method of ethylene oxide is provided which employs the same catalyst.;COPYRIGHT: (C)2008,JPO&INPIT
机译:解决的问题:提供一种可以生产具有高活性和选择性的环氧乙烷的催化剂,并提供一种使用相同的催化剂通过含分子氧的气体对乙烯进行气相氧化而制备环氧乙烷的方法。环氧乙烷生产用催化剂是通过以α-Al 2 O 3 为主要成分的载体载体得到的,其中红外吸收光谱的强度在在KBr压片法测定的红外吸收光谱中,波数为3,150 cm至3,800 cm -1 的范围基本为零。提供了使用相同催化剂的环氧乙烷的生产方法。;版权所有:(C)2008,日本特许会计师事务所

著录项

  • 公开/公告号JP4747066B2

    专利类型

  • 公开/公告日2011-08-10

    原文格式PDF

  • 申请/专利权人 株式会社日本触媒;

    申请/专利号JP20060272311

  • 发明设计人 三河 雅嗣;柚木 弘己;廣田 博之;

    申请日2006-10-03

  • 分类号B01J23/66;C07D301/10;C07D303/04;C07B61/00;

  • 国家 JP

  • 入库时间 2022-08-21 18:17:43

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号