PROBLEM TO BE SOLVED: To provide a method of molding a polylactic acid resin composition having an excellent heat resistance and its molding.;SOLUTION: The method of molding the polylactic acid resin composition including the step of repeating quick heating and quick cooling of the surface of a mold cavity comprises the steps of feeding a polylactic acid resin composition improved in crystallization speed into the cavity with a surface temperature of 90-140°C, holding the state for 5-60 seconds for crystallization, quickly cooling the cavity surface to 40-80°C, holding the state for 5-30 seconds and taking out the molding. The polylactic acid resin composition molding is obtained by this molding method and has a heat resistance temperature of ≥110°C.;COPYRIGHT: (C)2006,JPO&NCIPI
机译:解决的问题:提供一种成型具有优异耐热性的聚乳酸树脂组合物的方法及其成型方法;解决方案:成型聚乳酸树脂组合物的方法包括重复对表面进行快速加热和快速冷却的步骤模腔的制造包括以下步骤:将结晶速度提高了的聚乳酸树脂组合物以90-14℃的表面温度送入模腔,保持5-60秒的结晶状态,将模腔表面快速冷却至40 -80℃,保持该状态5-30秒并取出模制品。聚乳酸树脂组合物模制法是通过这种模制方法获得的,其耐热温度为110℃。COPYRIGHT:(C)2006,JPO&NCIPI

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号