(1) as for olefin resin (A), melt mass flow rate to be the ethylene resin of 0.5 - 10g/10 minute the constituent

机译:(1)烯烃树脂(A)的熔融质量流量为构成0.5〜10g / 10分钟的乙烯树脂。

摘要

PROBLEM TO BE SOLVED: To obtain a composition comprising a raw material component which can be uniformly mixed even in melting and kneading by an extrusion molding machine, consequently, causing a uniform and stable graft reaction, capable of providing a modified olefin-based resin having high qualities and stability and to provide a method for producing the modified olefin-based resin having excellent qualities using the composition.;SOLUTION: This resin composition is characterized in that in a composition for a functional group-containing compound modified olefin-based resin comprising an olefin-based resin (A), a functional group-containing compound (B) and a radical generator (C) as main components, (1) the olefin-based resin (A) comprises 5-100 wt.% of a granular body having an average particle diameter (R1) (unit: mm) satisfying formula (a) 0.02≤R1≤2.0 and 95-0 wt.% of the rest of a pellet body having an average particle diameter (R2) (unit: mm) satisfying formula (b) 2.0R2≤7.0 and (2) the functional group-containing compound (B) is solid at ordinary temperature (15°C). This method for producing the modified olefin-based resin is provided.;COPYRIGHT: (C)2002,JPO
机译:解决的问题:为了得到包含原料成分的组合物,所述原料成分即使通过挤出成型机进行熔融混炼也能够均匀地混合,因此能够引起均匀且稳定的接枝反应,从而能够提供具有以下特征的改性烯烃系树脂。高质量和高稳定性,并提供使用该组合物生产具有优良品质的改性烯烃基树脂的方法。解决方案:该树脂组合物的特征在于,在用于含官能团化合物的组合物中,改性烯烃基树脂包含烯烃基树脂(A),含官能团的化合物(B)和自由基产生剂(C)作为主要成分,(1)烯烃基树脂(A)占颗粒的5-100重量%。具有满足式(a)的平均粒径(R1)(单位:mm)的主体和具有平均粒径(R2)(单位:μm)的粒料主体的其余部分的0.02〜R12.0和95-0重量%。 mm)满足公式(b)2.0 < R 2和7.0和(2)含官能团的化合物(B)在常温(15℃)下为固体。提供了一种生产改性烯烃基树脂的方法。版权所有:(C)2002,JPO

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号