首页> 外国专利> Method of joining steel members, joining force enhancement method in the assembly consisting of steel members, die-casting products and steel products

Method of joining steel members, joining force enhancement method in the assembly consisting of steel members, die-casting products and steel products

机译:钢构件的接合方法,由钢构件,压铸产品和钢产品组成的组件中的接合力增强方法

摘要

Providing steel member preparation step the steel members of the two, in a state of butting the predetermined joining surface of the steel member 2, the method of bonding the steel member of the present invention, while being pressed under a pressure given the steel members of two by heating the bondable first temperature steel two members, the joint body forming step of forming a conjugate, after heating to a second temperature of A 1 transformation point or more in the steel member assembly, the A 1 By conditions to be applied 5 hours to lowered to 600 ℃ from the transformation point, and slowly cooled to a third temperature of 600 ℃ following the assembly, in this order and the bonding force strengthening step to strengthen the bonding force in the assembly including. Therefore, according to the joining method of the steel member of the present invention, it is possible to obtain sufficiently high bonding strength even when manufacturing a bonded body by bonding to each other steel members of two.
机译:提供钢构件准备步骤,在将钢构件2的预定接合表面对接的状态下,将本发明的钢构件接合的方法在将钢构件2的钢构件对接的状态下,在赋予钢构件2的压力下加压。两个通过加热可粘结的第一温度钢的两个构件,在共轭体形成步骤中形成共轭物,在钢构件组件中加热到第二个温度 1 转变点或更高后,A < Sub> 1 按条件施加5小时,从转变点降至600℃,并在组装后缓慢冷却至600℃的第三温度,以此顺序和结合力增强步骤来强化组件中的结合力包括。因此,根据本发明的钢构件的接合方法,即使在通过将两个钢构件彼此接合而制造接合体的情况下,也可以获得足够高的接合强度。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号