The invention relates to coke chemical production, and more specifically it relates to compositions for producing metallurgical coke. A charge for obtaining metallurgical coke, with an optimized proportion of components of regular coals of various ranks, containing: (25 - 65) % b.w. fat or gas fat coals and (35 - 75) % b.w. low-coking caking coals; or (25 - 65) % b.w. fat or gas fat coals and (35 - 75) % b.w. weak coking coals; or (25 - 40) % b.w. fat coals, (35 - 60) % b.w. low-coking caking coals and (5 - 35)% b.w. weak coking coals; or (30 - 55) % b.w. gas fat coals, (30 - 60) % b.w. low-coking caking coals and (5 - 20)% b.w. weak coking coals; or (35 - 40) % b.w. fat coals, (5 - 15) % b.w. gas fat coals and (50 - 55)% b.w. low-coking caking coals; or (10 - 30) % b.w. fat coals, (20 - 30) % b.w. gas fat coals, (20 - 60)% b.w. low-coking caking coals and (5 - 25) % b.w. weak coking coals.
机译:本发明涉及焦炭化学生产,更具体地说,涉及用于生产冶金焦的组合物。一种用于获得冶金焦的装料,其具有各种等级的普通煤的最佳成分比例,其中包括:(25-65)%b.w.脂肪或气态脂肪煤和(35-75)%b.w.低焦化结块煤;要么(25-65)%b.w.脂肪或气态脂肪煤和(35-75)%b.w.弱焦煤;要么(25-40)体重百分比脂肪煤,(35-60)%b.w.低焦化结块煤和(5-35)%b.w.弱焦煤;要么(30-55)%b.w.瓦斯脂肪煤,(30-60)%b.w.低焦化结块煤和(5-20​​)%b.w.弱焦煤;要么(35-40)%b.w.脂肪煤,(5-15)%b.w.瓦斯脂肪煤和(50-55)%b.w.低焦化结块煤;要么(10-30)体重百分比脂肪煤,(20-30)%b.w.瓦斯脂肪煤,(20-60)%b.w.低焦化结块煤和(5-25)%b.w.弱焦煤。

著录项

  • 公开/公告号EP2103667A4

    专利类型

  • 公开/公告日2011-05-25

    原文格式PDF

  • 申请/专利权人 MUSOKHRANOV BORIS;

    申请/专利号EP20070730439

  • 发明设计人 MUSOKHRANOV BORIS;

    申请日2007-04-10

  • 分类号C10B57/04;

  • 国家 EP

  • 入库时间 2022-08-21 17:57:39

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号