首页> 外国专利> METHOD FOR PREPARING POLY (DIPHENYL ETHER SULFONE) AND POLY (DIPHENYL ETHER DIPHENYL SULFONE) TERNARY POLYMER

METHOD FOR PREPARING POLY (DIPHENYL ETHER SULFONE) AND POLY (DIPHENYL ETHER DIPHENYL SULFONE) TERNARY POLYMER

机译:聚(二苯醚二甲砜)和聚(二苯醚二苯甲砜)三元共聚物的制备方法

摘要

A method for preparing poly(diphenyl ether sulfone) and poly(diphenyl ether diphenyl sulfone) ternary polymer comprises: adding high temperature organic solvent, stirring and heating; sequentially adding 4,4'-dihydroxydiphenyl, 4,4'-dichlorodiphenyl sulfone and 4,4'-dichlorophenyl diphenyl sulfone; after all the monomers are completely dissolved, heating to 100℃ and adding alkali metal carbonate salt-forming agent which is 5-10 mol % more than the amount of 4,4'-dihydroxy diphenyl added, and subsequently adding xylene; continuously heating and salt-forming reaction begins, and controlling the temperature at 190~210℃; then heating to 230~236℃, maintaining for 3-4 hours, finishing polymerization reaction and obtaining polymer viscous liquid; refining and obtaining the ternary polymer.
机译:一种制备聚二苯醚砜和聚二苯醚二苯砜三元聚合物的方法,包括:加入高温有机溶剂,搅拌并加热;依次加入4,4′-二羟基二苯基,4,4′-二氯二苯基砜和4,4′-二氯苯基二苯砜;所有单体完全溶解后,加热至100℃,加入碱金属碳酸盐成盐剂,该成盐剂比4,4'-二羟基二苯基的加入量增加5-10mol%,然后加入二甲苯。连续加热并开始成盐反应,并将温度控制在190〜210℃。然后加热至230〜236℃,保持3-4小时,完成聚合反应,得到聚合物粘稠液体。精制并获得三元聚合物。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号