首页> 外国专利> protect eco-friendly method of producing concrete mortar which acts to give a natural ecosystem . Use mortar to the concrete construction methods and eco- friendly nature -friendly way to configure the block for restoring the natural ecosystem constructed language seconds Combine stepped eco ecology and retaining wall blocks that make up the way to pave the way for action to prevent freezing eco -friendly and natural way configuration information to the natural eco -friendly and eco-friendly method of Civil hobakdol that apply to here

protect eco-friendly method of producing concrete mortar which acts to give a natural ecosystem . Use mortar to the concrete construction methods and eco- friendly nature -friendly way to configure the block for restoring the natural ecosystem constructed language seconds Combine stepped eco ecology and retaining wall blocks that make up the way to pave the way for action to prevent freezing eco -friendly and natural way configuration information to the natural eco -friendly and eco-friendly method of Civil hobakdol that apply to here

机译:保护生产混凝土砂浆的生态友好方法,该方法可赋予天然生态系统。将砂浆用于具体的施工方法和生态友好的自然友好方式来配置用于恢复自然生态系统构造语言的块秒,结合阶梯状生态和挡墙块,为行动以防止冻结生态铺平道路友好和自然的方式配置信息,适用于此处的民间霍巴克多的自然生态和环保方法

摘要

PURPOSE: a kind of manufacture environment-friendly concrete mortar, environmental-friendly biodegradable block, the manufacturing method of structure block, a kind of environmental-friendly armor stone, environmentally friendly boulder is to reduce toxicity concrete mortar, by introducing robber's balloon or the rod-shaped container of vinyl. ;CONSTITUTION: a kind of one end for being produced by high frequency fusion or combining s of container, vinyl, resin or robber's roller. 10-50 weight) mixed liquor, container is filled by the oxalic acid of 10-50 weight % or the water containing acid solution and 50-90 weight % of hydrochloric acid or the water of 10-50 weight ratios. In addition the air of 50-90 weight % is filled. One end of container is by scorification or indentation sequence mixing liquid and air, to obtain a final container. The cement of 40-65 weight %, 5-40 weight) sand and 5-30 weight % water mixing obtain mortar. Container is introduced into mortar. ;The 2011 of copyright KIPO submissions
机译:用途:一种制造环保混凝土砂浆,环保可生物降解的砌块,结构砌块的制造方法,一种环保装甲石,一种环保巨石是通过引入强盗气球或通过减少劫持来降低混凝土砂浆的毒性的方法。棒状的乙烯基容器。 ;组成:一种通过高频熔合或将容器,乙烯基,树脂或强盗辊组合而成的一端。 10-50重量%的混合液,用10-50重量%的草酸或含水酸溶液和50-90重量%的盐酸或10-50重量比的水填充容器。另外,填充50-90重量%的空气。容器的一端是通过胶凝或压痕顺序混合液体和空气,以获得最终的容器。将40-65重量%,5-40重量%的沙子和5-30重量%的水混合的水泥得到砂浆。将容器引入砂浆中。 ; 2011年版权KIPO提交文件

著录项

  • 公开/公告号KR20110027743A

    专利类型

  • 公开/公告日2011-03-16

    原文格式PDF

  • 申请/专利权人 HAN SANG KWAN;

    申请/专利号KR20110017496

  • 发明设计人 HAN SANG KWAN;

    申请日2011-02-28

  • 分类号C04B28/00;E02B3/14;E01C7/10;B28B7/00;

  • 国家 KR

  • 入库时间 2022-08-21 17:52:20