首页> 外国专利> POLARIZING PLATE AND MANUFACTURING METHOD THEREOF IN WHICH A POLARIZER AND PROTECTION FILM WITH DIFFERENT PERMEABILITY ARE MERGED WITH ADHESIVE MATERIALS OF DIFFERENT BONDING TIME WITH RESPECT TO A UNIT AREA AT EACH SPECIFIC TEMPERATURE

POLARIZING PLATE AND MANUFACTURING METHOD THEREOF IN WHICH A POLARIZER AND PROTECTION FILM WITH DIFFERENT PERMEABILITY ARE MERGED WITH ADHESIVE MATERIALS OF DIFFERENT BONDING TIME WITH RESPECT TO A UNIT AREA AT EACH SPECIFIC TEMPERATURE

机译:极化板及其制造方法,其中在每个特定温度下,针对单位面积,将具有不同磁导率的极化膜和保护膜与不同粘结时间的胶粘剂融合在一起

摘要

PURPOSE: A polarizing plate and a manufacturing method thereof are provided to minimize difference in adhesion time in order to maintain balance of the adhesion time, thereby suppressing curl generation.;CONSTITUTION: A polarizing plate is comprised of by laminating a protection film with first vapor permeability, a first water based adhesive layer, a polarizer, a second water based adhesive layer, and the protection film. The first water based adhesive layer is comprised of poly vinyl alcohol resin and polyamide epoxy resin with a weight ratio of 1 to 1 - 1 to 7. The second water based adhesive layer is comprised of poly vinyl alcohol resin and polyamide epoxy resin with the weight ratio of 1 to 0.05 - 1 to 1.;COPYRIGHT KIPO 2012
机译:用途:提供一种偏振片及其制造方法,以最小化粘合时间的差异,以保持粘合时间的平衡,从而抑制卷曲的产生。渗透性,第一水基粘合剂层,偏振器,第二水基粘合剂层和保护膜。第一水基粘合剂层由重量比为1-1至1至7的聚乙烯醇树脂和聚酰胺环氧树脂构成。第二水基粘合剂层由重量比为1的聚乙烯醇树脂和聚酰胺环氧树脂构成。 1:0.05-1:1的比例; COPYRIGHT KIPO 2012

著录项

  • 公开/公告号KR20110119325A

    专利类型

  • 公开/公告日2011-11-02

    原文格式PDF

  • 申请/专利权人 DONGWOO FINE-CHEM CO. LTD.;

    申请/专利号KR20100038958

  • 发明设计人 YOO JEONG HO;SONG IN KYU;YOO MIN KEUN;

    申请日2010-04-27

  • 分类号G02B5/30;C09J9/00;

  • 国家 KR