首页> 外国专利> A ASPHALT MIXTURE USING SBS

A ASPHALT MIXTURE USING SBS

机译:使用SBS的沥青混合料

摘要

The present invention relates to a reproduction modified asphalt mixtures with SBS, the lungs are discarded virgin asphalt and asphalt even with a mixture doemeuro exhibit a reliable quality similar to that of using only virgin asphalt an effect of reducing the production cost of the asphalt concrete with preventing environmental pollution due to the re-use of the recycled aggregates . ; this invention of the modifier , the weight-average molecular weight of 50,000 ~ 100,000 and a low molecular weight SBS 1 ~ 20 % by weight , a weight average molecular weight of 150,000 to 200,000 and the increment chair SBS 5 ~ 25 wt% , the polymer having a weight-average molecular weight of 300,000 ~ 350,000 SBS 10 ~ 35 wt. % and , from 1 to 10 % by weight process oil , petroleum resin 5 to 15% by weight , the antioxidant is 0.1 to 0.5 % by weight , characterized by a composition comprising a slurry oil yirum 20 to 40% by weight is used as an additive playing .
机译:本发明涉及一种具有SBS的再生改性沥青混合料,其肺部被丢弃为原始沥青,即使混合的doemeuro表现出与仅使用原始沥青相同的可靠质量,也降低了沥青混凝土的生产成本。防止由于回收的骨料的再利用而造成的环境污染。 ;本发明的改性剂,重均分子量为50,000〜100,000,低分子量SBS为1〜20重量%,重均分子量为15万〜200,000,增量椅SBS为5〜25重量%,重均分子量为300,000〜350,000 SBS 10〜35 wt。的组合物的含量为1%至10%(重量),5至15%(重量)的石油树脂,0.1至0.5%(重量)的抗氧化剂,其特征在于包含20至40%(重量)的浆料产量的油脂。加法演奏。

著录项

  • 公开/公告号KR101032697B1

    专利类型

  • 公开/公告日2011-05-06

    原文格式PDF

  • 申请/专利权人

    申请/专利号KR20090090402

  • 发明设计人 김병채;

    申请日2009-09-24

  • 分类号C08L95/00;

  • 国家 KR

  • 入库时间 2022-08-21 17:50:20