Method for laminating plate-shaped elements, comprises connecting a meltable adhesive layer of three material layers in an evacuatable laminating chamber with a flat heating device

机译:层压板状元件的方法,包括在可抽气的层压室内用平面加热装置连接三层材料的可熔融粘合剂层

摘要

The method for laminating plate-shaped elements, comprises connecting a meltable adhesive layer of three material layers in an evacuatable laminating chamber with a flat heating device at 135-160[deg] C. The layers remain after the generation of a vacuum in the laminating chamber without application of a mechanical pressure of 600-1200 mbar during a time tD of 50-180 seconds and the mechanical pressure is applied on the elements under holding the vacuum during a time tC of 400-900 seconds. The elements are held during the time tD in an interval from the heating device. The method for laminating plate-shaped elements, comprises connecting a meltable adhesive layer of three material layers in an evacuatable laminating chamber with a flat heating device at 135-160[deg] C. The layers remain after the generation of a vacuum in the laminating chamber without application of a mechanical pressure of 600-1200 mbar during a time tD of 50-180 seconds and the mechanical pressure is applied on the elements under holding the vacuum during a time tC of 400-900 seconds. The elements are held during the time tD in an interval from the heating device. After the progress of time tD and before beginning the time tC, the elements are in contact with the heating device during a time tP of 0-100 seconds. The elements are charged during the time tP with a mechanical pressure of 4-10 mbar and the pressure of 600-1200 mbar is applied on the element.
机译:层压板状元件的方法包括在可抽空的层压室中用135-160℃的平面加热装置连接三层材料的可熔融粘合层。在层压中产生真空后,这些层仍然保留在50-180秒的时间tD内不施加600-1200 mbar的机械压力,并且在400-900秒的时间tC内保持真空状态下将机械压力施加到元件上。在时间tD内,元件与加热设备之间保持一定间隔。层压板状元件的方法包括在可抽空的层压室中用135-160℃的平面加热装置连接三层材料的可熔融粘合层。在层压中产生真空后,这些层保留在50-180秒的时间tD内不施加600-1200 mbar的机械压力,并且在400-900秒的时间tC内保持真空状态下将机械压力施加到元件上。在时间tD内,元件与加热设备之间保持一定间隔。在时间tD经过之后并且在时间tC开始之前,元件在0-100秒的时间tP内与加热装置接触。在时间tP期间,对元件充电的机械压力为4-10 mbar,在元件上施加的压力为600-1200 mbar。

著录项

  • 公开/公告号CH701494A1

    专利类型

  • 公开/公告日2011-01-31

    原文格式PDF

  • 申请/专利权人 3S SWISS SOLAR SYSTEMS AG;

    申请/专利号CH20090001145

  • 发明设计人 RONALD LANGE;JUERG ZAHND;

    申请日2009-07-21

  • 分类号B32B37/18;B32B17/10;C03C27/12;H01L31/048;

  • 国家 CH

  • 入库时间 2022-08-21 17:48:11

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号