首页> 外国专利> Method for modifying e.g. medium density fiber board, involves maintaining maximum temperature over time period of specific hours and cooling thermal chamber or pressure tank at ambient temperature

Method for modifying e.g. medium density fiber board, involves maintaining maximum temperature over time period of specific hours and cooling thermal chamber or pressure tank at ambient temperature

机译:修改例如中密度纤维板,涉及在特定小时内保持最高温度,并在环境温度下冷却热室或压力罐

摘要

The method involves heating a thermal chamber (1) or a pressure tank up to maximum temperature in a temperature range from 150 to 220 degree Centigrade, where heating time is of 1-10 minutes per Kelvin. The maximum temperature is maintained over a time period of 1-8 hours. The thermal chamber or the pressure tank is cooled at ambient temperature, where cooling time is of 1-10 minutes per Kelvin. The thermal chamber or the pressure tank is equipped with a device that regulates humidity in the thermal chamber or the pressure tank.
机译:该方法包括在150至220摄氏度的温度范围内将热室(1)或压力罐加热至最高温度,其中每开尔文的加热时间为1-10分钟。最高温度保持1-8小时。热室或压力罐在室温下冷却,每开尔文的冷却时间为1-10分钟。热室或压力罐配备有调节热室或压力罐中湿度的装置。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号