PROBLEM TO BE SOLVED: To provide a laminated coating film of an automobile body that has a high ground concealing property and high appearance, a coating method of the automobile body for reducing the running cost, and the automobile body having the laminated coating film.;SOLUTION: In this laminated coating film of the automobile body, the coating method of the automobile body, and the automobile body having the laminated coating film, an electrodeposition coating film, a first middle coating film, a second middle coating film, a base coating film, and a clear coating film are stacked on a metal substrate in that order. A first middle coating material constituting the first middle coating film and a second middle coating material constituting the second middle coating film are acid epoxy curing middle coating materials containing acrylic resin containing a carboxyl group whose acid value is 50-300 mgKOH/g (solid content) and carboxylic acid ester group, and acrylic resin containing an epoxy group whose epoxy group equivalence is 50-700. The first middle coating material contains a coloring pigment and extender pigment as a pigment, and the second middle coating material contains no pigment or contains only an extender pigment as a pigment.;COPYRIGHT: (C)2012,JPO&INPIT
机译:解决的问题:提供一种具有高地面遮盖性和高外观的车身的层压涂膜,降低运行成本的车身的涂覆方法以及具有该层压涂膜的车身。解决方案:在该车身的层压涂膜中,车身的涂覆方法以及具有该层压涂膜的汽车车身,电沉积涂膜,第一中间涂膜,第二中间涂膜,底涂层膜和透明涂膜以此顺序堆叠在金属基板上。构成第一中间涂层膜的第一中间涂层材料和构成第二中间涂层膜的第二中间涂层材料是酸环氧固化的中间涂层材料,其包含具有酸值为50-300 mgKOH / g(固体成分)的羧基的丙烯酸树脂。 )和羧酸酯基,以及含有环氧基为50-700的环氧基的丙烯酸树脂。第一种中间涂料包含着色颜料和增量颜料作为颜料,第二种中间涂料不含颜料或仅包含增量颜料作为颜料。;版权所有:(C)2012,JPO&INPIT

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号