PPROBLEM TO BE SOLVED: To provide a flexible polyurethane foam which is easy in adjustment of raw material formulation and molding and has outstanding low hardness and low strain, and to provide a method for producing the same. PSOLUTION: The flexible polyurethane foam has a hardness as measured in accordance with JIS K 6400 of 10-30 N and a compression residual strain of 2-6%. For producing the foam, a foam raw material comprising a polyol, a polyisocyanate, a catalyst, and a foaming agent is reacted and foamed by a molding process. The polyol is a polyether polyol prepared by adding propylene oxide or ethylene oxide to a polyol which has a mass average molecular weight of 4,000-6,000 and is bifunctional or trifunctional with respect to a hydroxy group, and the content of ethylene oxide in the polyol is 15-30 mass%. The polyisocyanate is blended so that it has an isocyanate index of 90-110. In addition, the raw material comprises a plasticizer. PCOPYRIGHT: (C)2008,JPO&INPIT
机译:

要解决的问题:提供一种易于调整原料配方和成型并且具有优异的低硬度和低应变的柔性聚氨酯泡沫,并提供一种生产该聚氨酯泡沫的方法。

解决方案:所述软质聚氨酯泡沫具有根据JIS K 6400测得的10-30 N的硬度和2-6%的压缩残余应变。为了生产泡沫,使包含多元醇,多异氰酸酯,催化剂和发泡剂的泡沫原料通过成型工艺反应并发泡。多元醇是通过将环氧丙烷或环氧乙烷添加到质均分子量为4,000-6,000且相对于羟基为双官能或三官能的多元醇中而制备的聚醚多元醇,并且环氧乙烷在多元醇中的含量为15-30质量%。共混多异氰酸酯,使其异氰酸酯指数为90-110。另外,原料包括增塑剂。

版权:(C)2008,日本特许厅&INPIT

著录项

  • 公开/公告号JP5032817B2

    专利类型

  • 公开/公告日2012-09-26

    原文格式PDF

  • 申请/专利号JP20060265237

  • 发明设计人 和田 浩孝;

    申请日2006-09-28

  • 分类号C08G18/48;C08G18/65;C08K5/00;C08L75/04;C08G101/00;

  • 国家 JP

  • 入库时间 2022-08-21 17:40:01

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号