Hydrophilic photocatalyst, which is proposed to obtain titanium dioxide anatase photocatalytic effect and excellent chromium on a substrate (TiO 2) film and a manufacturing method thereof, the present invention, the temperature of the substrate more by coating the (TiO 2) film of titanium dioxide which was coated (TiO 2) thin film amorphous titanium dioxide in a state of being maintained at 200 ℃ or less, with a pure anatase type titanium dioxide (TiO 2) film directly above, anatase by coating silicon dioxide (SiO 2) thin films of titanium dioxide mold (TiO 2) film directly above, super-hydrophilicity of 10 ° or less is a photocatalytic effect in response to UV irradiation appeared within one hour, and water hydrophilic photocatalyst titanium dioxide (TiO 2) thin film is coated on a chromium substrate having a characteristic hydrophilicity of 20 ° or less is maintained up to 18 hours contact angle and its manufacturing method. None [Selection Figure]
机译:提出了一种亲水性光催化剂,其旨在在基材(TiO 2)膜上获得二氧化钛锐钛矿型的光催化效果和优异的铬及其制造方法,本发明通过涂覆该基材进一步提高基材的温度(TiO 2)的二氧化钛膜,以纯锐钛矿状态保持在(TiO 2)薄膜无定形二氧化钛,保持在200℃以下型二氧化钛(TiO 2)膜正上方,通过涂覆二氧化硅(SiO 2)二氧化钛模具(TiO 2)薄膜的锐钛矿>薄膜正上方,超亲水性在10°或以下是在1小时内出现对紫外线辐射的光催化作用,并且将亲水性光催化剂二氧化钛(TiO 2)薄膜涂覆在具有20°或20以下的亲水性的铬基板可保持长达18小时的接触角及其操作制造方法。无[选择图]

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号