PPROBLEM TO BE SOLVED: To provide a doped ceria-based sintered body being dense, having a uniform structure in a nano level and having high electroconductive characteristics and to provide its producing method. PSOLUTION: The rare earth element-doped nano ceria-based sintered body is characterized by having a relative density of 95% or more, an average particle diameter of 110SP2/SPnm or more and 210SP2/SPnm or less and a standard deviation () expressing the spread of a particle diameter distribution of 610 nm or less. PCOPYRIGHT: (C)2009,JPO&INPIT
机译:<解决的问题:提供一种致密的掺杂的基于二氧化铈的烧结体,其在纳米水平上具有均匀的结构并且具有高的导电特性,并且提供了其制造方法。

解决方案:掺杂稀土元素的纳米二氧化铈基烧结体的特征在于相对密度为95%或更高,平均粒径为110 2 nm且210 < SP> 2 nm以下,并且标准偏差()表示610 nm以下的粒径分布的扩展。

版权:(C)2009,日本特许厅&INPIT

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号