首页> 外国专利> Methods for precipitating iron and arsenic in the form of low soluble compounds, including iron oxide and arsenic, standardize confidence/As of 1-3.5 and pH of 1.5-4.5 to precipitate organic arsenic, and feed the precipitate into hydrogen energy conversion at 150-200 degrees Celsius for the purpose of Get the crystal scorpion.

Methods for precipitating iron and arsenic in the form of low soluble compounds, including iron oxide and arsenic, standardize confidence/As of 1-3.5 and pH of 1.5-4.5 to precipitate organic arsenic, and feed the precipitate into hydrogen energy conversion at 150-200 degrees Celsius for the purpose of Get the crystal scorpion.

机译:以低可溶性化合物(包括氧化铁和砷)形式沉淀铁和砷的方法,将置信度/ As设置为1-3.5,pH值设置为1.5-4.5,以沉淀有机砷,然后将沉淀物进料到150- 200摄氏度的目的是获取水晶蝎子。

摘要

Method for precipitating Arsenic and iron in the form of a poorly soluble Compound,That includes an oxidizing Solution containing Iron and Arsenic containing solution by means of an Oxidant, with a ratio of 1 - Faith - as a pH 3.5 and 1.5 - 4.5And send the precipitated a hydrothermal conversion to 150 - 200 degrees Celsius.
机译:沉淀难溶性化合物形式的砷和铁的方法,该方法包括通过氧化剂以1-信念-pH 3.5和1.5-4.5的比例将含铁和含砷溶液氧化的溶液沉淀物将水热转化为150-200摄氏度。

著录项

  • 公开/公告号CL2011002032A1

    专利类型

  • 公开/公告日2012-02-03

    原文格式PDF

  • 申请/专利权人 OUTOTEC OYJ;

    申请/专利号CL20110002032

  • 申请日2011-08-19

  • 分类号C01G28/02;C01G49/00;C02F1/02;

  • 国家 CL

  • 入库时间 2022-08-21 17:25:20

相似文献

  • 专利
  • 外文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号