A method and distance are used to produce reduced iron in a vertical reactor, the upper reduction zone and the lower reduction zone of the reactor.

机译:一种方法和距离用于在立式反应器,反应器的上部还原区和下部还原区中生产还原铁。

摘要

Method for producing iron in vertical reactor comprising Heat recovered in Higher gas heating Unit, feed Forming unit which contains Coal volatileDevolatilizar and REACT with higher gas recovered, Feed and Feed gas desulphurisation Agent, Heat higher centrifugal separator; and installation.
机译:在立式反应器中生产铁的方法,包括:在较高气体加热单元中回收的热量,包含煤挥发物的挥发物形成单元和高回收率的REACT以及较高回收率的气体,进料和原料气脱硫剂,加热较高的离心分离器。和安装。

著录项

  • 公开/公告号CL2011002459A1

    专利类型

  • 公开/公告日2012-04-20

    原文格式PDF

  • 申请/专利权人 PAUL WURTH S.A.;

    申请/专利号CL20110002459

  • 发明设计人 ROTH JEAN LUC;RODRIGUEZ DAVID;

    申请日2011-10-03

  • 分类号C21B13/02;

  • 国家 CL

  • 入库时间 2022-08-21 17:25:21