Injection molded automotive component made from polyester composites, comprising of at least a polyester, glass filler, epoxy additive, antistatic agents, thermal stabilizers, process stabilizers and antioxidant additives; wherein polyester composite comprises combination at least two different IV of polyesters, preferably recycled poly ethylene terephthalate (RPET) resin 55-92% by weight and the RPET resin having the IV range from 0.1 - 1.5; wherein these two IVs are from two different consumer used sources, one IV is from PET bottles and another IV is from non bottle source like PET films and fibers; wherein most optimized range of glass filler (silica fibers) is 22 - 36 % by weight; wherein epoxy additive of low molecular weight (100 to 3000 gram/mole) is 0.05 to 3% by weight; wherein antistatic agents are from metal alkyl sulphonate derivatives and is 0.02 to 5% by weight; wherein process stabilizer is 0.05 to 1% by weight of stearate based additive.
机译:由聚酯复合材料制成的注塑汽车部件,至少包括聚酯,玻璃填料,环氧添加剂,抗静电剂,热稳定剂,过程稳定剂和抗氧化剂添加剂;其中聚酯复合材料包含至少两种不同IV的聚酯的组合,优选IV-55重量%至92重量%的再循环的聚对苯二甲酸乙二醇酯(RPET)树脂和IV为0.1-1.5的RPET树脂;其中这两个静脉注射液来自两种不同的消费者使用来源,一个静脉注射液来自PET瓶,另一个静脉注射液来自非瓶状来源,如PET薄膜和纤维。其中玻璃填料(二氧化硅纤维)的最优化范围是22-36重量%;其中低分子量(100至3000克/摩尔)的环氧添加剂为0.05至3重量%;其中抗静电剂来自烷基磺酸金属盐衍生物,重量比为0.02-5%。其中过程稳定剂是硬脂酸酯基添加剂的0.05-1重量%。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号