Abstract A slag fuming process wherein a slag containing arsenic or arsenic and antimony together with zinc and lead is heated and reduced in a slag fuming furnace, and zinc and lead are separated by evaporation, characterized in that it comprises causing a copper melt containing copper in an amount being 5 to 100 wt % relative to that of the slag charged in the above furnace and being 100 wt % or more relative to that of the lead contained in the above slag to be co-present in the above slag melt at a temperature of 1075 to 1500°C, and reacting the copper melt with arsenic or arsenic and antimony contained in the slag, to form a Cu-Fe-Pb-As based uniform melt. The above process of slag fuming and the like can be suitably employed for producing, by the use of a slag generated from a smelting furnace for refining zinc and/or lead, a dust containing zinc and lead and being reduced in the contents of arsenic and antimony, and a slag stably satisfying the environmental standard for soil, at a low treatment cost.
机译:摘要一种炉渣发烟过程,其中将含有砷或砷和锑以及锌和铅的炉渣在炉渣发烟炉中加热并还原,并通过蒸发将锌和铅分离,其特征在于,这导致在炉渣中形成含铜的铜熔体。相对于在上述炉中装入的炉渣的量为5至100wt%,并且相对于在温度下在上述炉渣熔体中共存的上述炉渣中所含的铅的量为100wt%以上温度为1075至1500℃,并使铜熔体与炉渣中所含的砷或砷和锑反应,形成基于Cu-Fe-Pb-As的均匀熔体。通过使用从熔炼炉产生的用于精炼锌和/或铅的炉渣,可以将上述炉渣发烟等方法适当地用于生产含锌和铅且降低了砷含量的粉尘。锑和稳定满足土壤环境标准的矿渣,且处理成本低。

著录项

  • 公开/公告号IN252394B

    专利类型

  • 公开/公告日2012-05-18

    原文格式PDF

  • 申请/专利权人

    申请/专利号IN2578/CHENP/2006

  • 申请日2006-07-14

  • 分类号C22B19/28;C22B19/32;C22B13/06;C22B19/04;C22B7/04;C22B5/16;C04B5;C22B19/30;C22B7;C22B13/02;

  • 国家 IN

  • 入库时间 2022-08-21 17:23:56

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号