首页> 外国专利> Bonded flux and solid wire for submerged arc welding, and method for submerged arc welding of steel for low temperature service

Bonded flux and solid wire for submerged arc welding, and method for submerged arc welding of steel for low temperature service

机译:埋弧焊用药芯焊丝和实心焊丝,以及低温工作用钢的埋弧焊方法

摘要

Disclosed is a bonded flux and a solid wire for submerged arc welding, and a method for submerged arc welding of a low-temperature steel each of which gives a weld bead (weld metal) having excellent low-temperature fracture toughness with satisfactory weldability. The bonded flux includes 23-43% of MgO, 11-31% of Al2O3, 6-16% of CaF2,7-20°% of SiO2, 1.0-8.0% as CO2 equivalent of a metal carbonate, a total of 2-16% of CaO and/or BaO, 0.4-1.5% of metallic silicon, a total of 1.0-7.0% as titanium equivalent of metallic titanium and titanium oxide, a total of 0.01-0.20% as boron equivalent of metallic boron and/or boron oxide, and a total of 1.0-6.0% as equivalents of respective elements of at least one oxide of Na, K, and Li, and has a ratio ([Total Ti]+[Total B])/[SiO2] of from 0.05 to 0.55.
机译:公开了一种用于埋弧焊的焊剂和实心焊丝,以及一种低温钢的埋弧焊方法,其各自给出了具有优异的低温断裂韧性且具有令人满意的可焊接性的焊道(焊缝金属)。键合助熔剂包括23-43%的MgO,11-31%的Al 2 O 3 ,6-16%的CaF 2 , SiO 2 的7-20 %%,CO 2 当量的金属碳酸盐的1.0-8.0%,CaO和/或BaO的总量为2-16%,金属硅的0.4-1.5%,金属钛和氧化钛的钛当量的总量为1.0-7.0%,金属硼和/或氧化硼的硼当量的总量为0.01-0.20%,以及1.0-作为Na,K和Li中至少一种氧化物的各元素当量的6.0%,并且([Total Ti] + [Total B])/ [SiO 2 ]之比为0.05至0.55。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号