MANUFACTURING METHOD OF A RESIST PRINTING MELAMINE RESIN AND A RESIST PRINTING MELAMINE SHEET MANUFACTURED BY USING THE METHOD CAPABLE OF IMPROVING FLAME RETARDANT CAPACITY CONSUMING RELATIVELY SMALL AMOUNT

机译:耐胶印三聚氰胺树脂的制造方法和使用能够提高相对阻燃量的方法制造的耐胶印三聚氰胺板的制造方法

摘要

PURPOSE: A manufacturing method of a resist printing melamine resin and a resist printing melamine sheet manufactured by using the method are provided to manufacture an improved resist printing melamine resin which maintains advantages of existing melamine resin and can be conveniently produced and used.;CONSTITUTION: A manufacturing method of a resist printing melamine resin comprises following steps: a pre-condensation step which adds formalin and melamine in a condition with pH 7-10 at less than 40deg.C and gradually increases temperature to 80-100deg.C; a condensation step which polycondenses the reactant in pH 7-10 at 80-100deg.C and adds a resist printing compound to the reactant. A molar ratio of the formalin and melamine is 1.4-2.1. 1-10 parts by weight of a resist printing melamine resin are added based on amount of the reactant.;COPYRIGHT KIPO 2012
机译:目的:提供一种抗蚀剂印刷三聚氰胺树脂的制造方法和使用该方法制造的抗蚀剂印刷三聚氰胺片,以制造改进的抗蚀剂印刷三聚氰胺树脂,其保留了现有三聚氰胺树脂的优点并且可以方便地生产和使用。抗蚀剂印刷三聚氰胺树脂的制造方法包括以下步骤:预缩合步骤,在低于40℃,pH 7-10的条件下添加福尔马林和三聚氰胺,并逐渐升高温度至80-100℃。缩合步骤,该缩合步骤在80-100℃下将pH 7-10的反应物缩聚,并向反应物中加入抗蚀剂印刷化合物。福尔马林与三聚氰胺的摩尔比为1.4-2.1。基于反应物的量添加1-10重量份的抗蚀剂印刷三聚氰胺树脂。; COPYRIGHT KIPO 2012

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号