FLAME-RETARDANT POLYESTER RESIN HAVING EXCELLENT DYEABILITY AND SHRINKAGE TOGETHER WITH GOOD POLYMERIZATION AND SPINNING PROPERTY, AND A MANUFACTURING METHOD THEREOF

机译:具有优良聚合性和纺丝性能的优异的可染性和收缩性的阻燃聚酯树脂及其制造方法

摘要

PURPOSE: A manufacturing method of flame-retardant polyester resin is provided to provide have dyeability to cation dye, to have excellent flame retardance together with excellent shrinkage, thereby using for manufacturing polyester fiber.;CONSTITUTION: A flame-retardant polyester resin is manufactured by polycondensation of terephthalic acid or ester-formable derivative thereof, and diol components under the presence of thermal stabilizer. The manufacturing method of polyester resin comprises: a step of adding 4.0-8.0 weight% of dicarboxylic acid in chemical formula 1having sulfonate group into an organic unit; a step of adding 1.0-4.0 weight% of polyalkylene glycol with the molecular weight of 400-6000 based on total diol components; and a step of adding a compound in chemical formula 2 in order to contain 1,000-10,000 ppm of phosphorus based on the weight of polyester resin.;COPYRIGHT KIPO 2012
机译:用途:提供一种阻燃性聚酯树脂的制造方法,以提供对阳离子染料具有可染性,同时具有出色的阻燃性和优异的收缩率,从而用于制造聚酯纤维。对苯二甲酸或其酯可形成的衍生物与二醇组分在热稳定剂存在下的缩聚反应。聚酯树脂的制造方法包括:在有机单元中添加4.0〜8.0重量%的具有磺酸酯基的化学式1的二羧酸的步骤。基于总二醇组分,添加1.0-4.0重量%的分子量为400-6000的聚亚烷基二醇的步骤;以及添加化学式2的化合物以使磷含量基于聚酯树脂的重量为1,000-10,000 ppm的步骤。; COPYRIGHT KIPO 2012

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号